Lead and Zinc ore Processing plant_Lead & Zinc Ore Beneficiation Plant_Lead&Zinc ore Flotation Technology
Place of Origin:Henan China (Mainland) | Brand Name:GHM | Model Number:flotation | Certificate:ISO9001-2008 |
Technology:Flotation | Service:whole using life | Installation:guid by engineer | Plant designing:supplying |
Spare parts:suppying | commissioning:supplying |
Lead&Zinc ore Processing plant_Lead&Zinc ore Beneficiation Plant_Lead&Zinc ore Flotation Technology
Lead&Zinc is mined either at open pit Lead&Zinc ore mines or underground Lead&Zinc ore mines. GHM can supply complete set of Lead&Zinc ore processing line.
Common equipment used for Lead&Zinc ore Processing:
Equipment commonly used for Lead&Zinc ore processing includes: jaw crusher, fine crusher, ball mill, electronic feeder, spiral classifier, mixing tank, flotation machine.
The models for each machine is based on production capacity.
GHM Flotation Production Process for Lead&Zinc Ore Selecting:
- 1. Crushing and Grinding stage
The extracted ore should be crushed by jaw crusher initially and then by fine crusher. When it gets the reasonable fineness, it is transported into ball mill by elevating conveyer and feeder, and is milled by ball mill.
- 2. Classifying stage
The subtle milled ore gets the next procedure: classification. There is a theory that if the weights of solid particles are different, the sedimentations will be different, and the mixed ore can be classified by screw classifier.
- 3. Mixing and Floatation stage
The classified ore gets into mixing tank for fully mixing. At this stage, chemical agent for foam can be added. After fully mixing, the slurry will enter into flotation machine.
When the floatation machine works, the motor drives the impeller to revolve, so the centrifugal effect and negative pressure are produced. On one hand, ample air is absorbed and mixed with mineral slurry, on the other hand, the mixed mineral slurry is mingled with additive, meanwhile, the foams are thinning, the mineral is bounded with foams, and floats up to the surface of mineral slurry and the mineralized foam is formed. The liquid surface can be adjusted with the height of adjustment flashboard, so that the useful foams are scraped with squeegee.
- 4. Concentrator thickening and drying
Then Lead&Zinc concentrate is separated from others. Since the separated ore are wet, they should be dewatered by thicker initially, and dried by dryer.
GHMthanks to our specialists in Sales, Technical, Engineering and Production Departments, each customer can benefit and enjoy our all- around professional supports on plant designing, equipment manufacturing, installation, commissioning, technical training and after- sales service. Welcome to “Good Heavy Machine”!
GHMthanks to our specialists in Sales, Technical, Engineering and Production Departments, each customer can benefit and enjoy our all- around professional supports on plant designing, equipment manufacturing, installation, commissioning, technical training and after- sales service.
Packaging Detail:Standard export package. |
Delivery Detail:40-50 days after in receipt of deposit |